Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EM2212 PC Automotive interiors. 10% glass-reinforced. Increased stiffness/structural ridigity. High modulus/ductile. Foamed skin instrument panel uses also. |
|||
Izod Impact, Notched | 2.13 J/cm @Temperature -30.0 °C |
3.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
Izod Impact, Notched | 2.13 J/cm @Thickness 6.40 mm |
3.99 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
Izod Impact, Notched | 2.13 J/cm @Temperature -30.0 °C |
3.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release. |
|||
Izod Impact, Notched | 2.13 J/cm @Thickness 6.40 mm |
3.99 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release. |
|||
Izod Impact, Notched | 2.13 J/cm @Thickness 3.17 mm |
3.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXG121R PC PC in special effects colors. ""Diamond Sparkle"" appearance additives. Color package may affect performance. |
|||
Izod Impact, Notched | >= 2.13 J/cm | >= 3.99 ft-lb/in | ASTM D256 |
Petromont 1202 High Density Polyethylene Resin Petromont HDPE 1202 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as shipping containers.. |
|||
Izod Impact, Notched | >= 2.13 J/cm | >= 3.99 ft-lb/in | ASTM D256 |
Petromont 4100 High Density Polyethylene Resin Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe
appl.. |
|||
Izod Impact, Notched | >= 2.13 J/cm | >= 3.99 ft-lb/in | ASTM D256 |
Petromont 5001 High Density Polyethylene Resin Petromont HDPE 5001 is a high-density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Izod Impact, Notched | 2.13 J/cm @Temperature -30.0 °C |
3.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Izod Impact, Notched | 2.13 J/cm @Temperature 23.0 °C |
3.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Izod Impact, Notched | 2.13 J/cm @Temperature 23.0 °C |
3.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton OV00A PPS (Asia Pacific) LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL ECN0240 PPE+PS (Asia Pacific) PPE+PS, Auto exterior grade |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3063UV-3120 Black, UV Stabilized Modified Polypropylene DescriptionPolyfort® FPP 3063UV-3120 is a black, UV stabilized, 30% chemically coupled, glass reinforced, high impact resistance, modified polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3063UV-3120 Black, UV Stabilized Modified Polypropylene DescriptionPolyfort® FPP 3063UV-3120 is a black, UV stabilized, 30% chemically coupled, glass reinforced, high impact resistance, modified polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3063UV-3120 Black, UV Stabilized Modified Polypropylene DescriptionPolyfort® FPP 3063UV-3120 is a black, UV stabilized, 30% chemically coupled, glass reinforced, high impact resistance, modified polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3063UV-3120 Black, UV Stabilized Modified Polypropylene DescriptionPolyfort® FPP 3063UV-3120 is a black, UV stabilized, 30% chemically coupled, glass reinforced, high impact resistance, modified polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3063UV-3120 Black, UV Stabilized Modified Polypropylene DescriptionPolyfort® FPP 3063UV-3120 is a black, UV stabilized, 30% chemically coupled, glass reinforced, high impact resistance, modified polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific) LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber. |
|||
Izod Impact, Notched | 2.13 J/cm @Temperature -30.0 °C |
3.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics PREVEX W20 PPE+PS Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |