Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Petromont 4100 High Density Polyethylene Resin Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe
appl.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | TM R050-36 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Celanese Vandar® 8000 PBT
(Unverified Data**) Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D 638 |
RTP Company RTP 600 FR AU Acrylonitrile Butadiene Styrene (ABS), Medium Impact - Flame Retardant - UV Stabilized - UL94 V-0 |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D 638 |
RTP Company RTP 661 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - EMI/RFI/ESD Protection |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | |
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Tensile Strength at Break | >= 34.5 MPa @Temperature 23.9 °C |
>= 5000 psi @Temperature 75.0 °F |
|
Master Bond UV15LV One Component, UV Curable Epoxy Based System Product Description: Master Bond UV15LV is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It has low viscosity and it is widely used in a variety of .. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100STL (COND, 50% RH) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D 638 |
RTP Company RTP 101 CC HI Polypropylene (PP), High Impact - Glass Fiber - Chemically Coupled |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | film; ASTM D882 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D 638 |
RTP Company ESD A 1000 Polybutylene Terephthalate (PBT), ESD Protection - Static Dissipative |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D 638 |
RTP Company RTP 1300 TFE 10 Polyphenylene Sulfide (PPS), PTFE Lubricated |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. polycarbonate; 20 s set time |
Elmer's Products Aron Alpha® 101 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Superior tensile and shear strengths, well suited for metal bondingLow gap fill. Methyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substr.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. polycarbonate; 20 s set time |
Elmer's Products Aron Alpha® 201 Cyanoacrylate Adhesive (Industrial Krazy Glue™) General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. rigid PVC; 3 s set time |
Elmer's Products Aron Alpha® 202F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. rigid PVC; 25 s set time |
Elmer's Products Aron Alpha® 203 Cyanoacrylate Adhesive (Industrial Krazy Glue™) General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair o.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. rigid PVC; 3 s set time |
Elmer's Products Aron Alpha® 212E Cyanoacrylate Adhesive (Industrial Krazy Glue™) For clean, fast applications. Best for high speed automated assembly.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous s.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. polycarbonate; 3 s set time |
Elmer's Products Aron Alpha® 231F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. rigid PVC; 5 s set time |
Elmer's Products Aron Alpha® 232 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. polycarbonate; 15 s set time |
Elmer's Products Aron Alpha® 253TX Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. rigid PVC; 5 s set time |
Elmer's Products Aron Alpha® 282F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | vs. polycarbonate; 60 s set time |
Elmer's Products Aron Alpha® 402X Cyanoacrylate Adhesive (Industrial Krazy Glue™) Engineered for high temperature and high impact resistance.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. .. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Celanese VANDAR 4602ZHR PBT, Unfilled 4602ZHR is an unfilled hydrolysis resistant PBT alloy with excellent thermal stability, toughness and weatherability characteristics.Information provided by Celanese |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Celanese VANDAR 8000 PBT, Unfilled Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | cured, grit-blasted steel; ASTM D2095 |
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B908 , 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D 638 |
RTP Company RTP 3003 Polymethylpentene (PMP), Glass Fiber |
|||
Tensile Strength at Break | 34.5 MPa | 5000 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | >= 34.5 MPa | >= 5000 psi | |
Master Bond EP3HTSMed Silver Filled, Medical Grade Epoxy Description: Master Bond EP3HTSMed is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast cure schedu.. |