Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent; ASTM D790 |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent; ASTM D790 |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-5052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin Features: Excellent balance of stiffness and toughness, low odor.Applications: Margarine and spreads, thin walled containers, frozen food containers.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Petromont 1202 High Density Polyethylene Resin Petromont HDPE 1202 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as shipping containers.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR350CS-01 Polypropylene Random Copolymer COPYLENE® CR350CS-01 is a clarified, reactor grade, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release for larger ar.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lidsFormolene LH5206 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 2.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer COPYLENE™ CM015 is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications: Injection M.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® C513UV HDPE Blow Molding Resin
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Outstanding impact resistanceExcellent ESCRExcellent processabilityUV stabilizationApplications: Intermediate bulk containersAgricultural containersInfor.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP502 Polypropylene Copolymer Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
M. Holland Company CP510 Polypropylene Copolymer Additives: Heat Stabilizer, Nucleating AgentsFeatures: High Flow, High Impact Resistance, Heat Stabilizer, NucleatedUses: Construction Applications, Lawn and Garden EquipmentApprovals: FDA 21 CFR 17.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2575N injection Molded Polypropylene Impact Copolymer for High Speed injection Molded ApplicationsFormolene® 2575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging, .. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent, 16:1 span:depth,0.5in/min; ASTM D790 |
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin Resin Type: Hexene CopolymerCharacteristics: Moderate flowExcellent impact strengthExcellent ESCRGood warpage resistanceApplications: Industrial partsSeatsFood and household containersAgricultural p.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent; 16:1 span:depth; 0.5 in/min; ASTM D790 |
Chevron Phillips Marlex® 9505H High Density Polyethylene This gas phase, high molecular weight, hexene copolymer with antistatic agent is tailored for lightweight blow molded containers that:Require outstanding ESCRRequire excellent impact resistanceAre d.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | Tangent; ASTM D790 |
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding This extra high molecular weight, hexane copolymer is tailored for intermediate bulk container applications that require:Outstanding impact resistanceOutstanding ESCRExcellent processabilityUV stabi.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow C719-35RNHP Polypropylene Resin DOW C719-35RNHP is intended for use in injection molding applications requiring a good impact/stiffness balance.Information provided by DowDow Announced Sale of Global Polypropylene Business to Bras.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% Secant; ASTM D790A |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790A |
Dow TF0807 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow 6D83K Polypropylene Resin DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July .. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6800WV Impact Copolymer Polypropylene Description: High Melt Flow, Nucleated, Excellent Mold Release, AntistaticApplications: Suggested Uses Include Housewares, Large Part Injection Molding, Thin-Walled Injection MoldingThis resin meets.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TR3020UC Random Copolymer Polypropylene Description: Maximum see-through clarity, minimal haze; superior color stability, process stability and gloss. Applications: Suggested uses include extrusion, blow molding, thermoforming, food cont.. |
|||
Flexural Modulus | >= 1.07 GPa | >= 155 ksi | ASTM D790 |
Buckeye Polymers BP RPP 1012 T BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM015G Polypropylene Impact Copolymer COPYLENE® CM015G is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications:Injection M.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Amco PRIMATOP HDPE 003946HP Blow Molding Polyethylene HDPE 003946HP features antistat, outstanding ESCR, and excellent impact resistance. Applications include detergent bottles, industrial containers, large parts, and household and industrial chemical .. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | 0.5 in/min, Tangent Method; ASTM D790 |
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.Former A-Top Polymers product; part of Amco product line since 2013.. |
|||
Flexural Modulus | 1.07 GPa | 155 ksi | ASTM D790 |
Chase Plastics CP Pryme® PPC100NB-10M Polypropylene Copolymer Information provided by Chase Plastics. |