Physical Properties Metric English Comments
ESCR 10% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F50; ASTM D1693
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b..
ESCR 10% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693-B
Petromont 1202 High Density Polyethylene Resin
Petromont HDPE 1202 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as shipping containers..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693-B
Petromont 4100 High Density Polyethylene Resin
Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe appl..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693-B
Petromont 5001 High Density Polyethylene Resin
Petromont HDPE 5001 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa..
ESCR 10% Igepal® 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
ESCR 10% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables
Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of go..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin
Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
Condition B, F50; ASTM D1693
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
This hexene copolymer is tailored for pipe applications that require:Good melt strengthGood pipe stiffnessOutstanding ESCRTypical corrugated pipe applications for HP076 include:Culverts and storm se..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693A
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693A
ExxonMobil Paxon™ 7004 Crosslinkable Rotational Molding Resin
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693A
ExxonMobil Paxon™ 7203 Crosslinkable Rotational Molding Resin
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693A
ExxonMobil Paxon™ 7204 Crosslinkable Rotational Molding Resin
Product Description: Paxon™ 7000 series of crosslinkable mHDPE resins are designed to offer outstanding ESCR, toughness, thermal, impact and notch failure resistance. These resins are ideally suite..
ESCR 10% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693, B
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin
Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
ESCR 10% Igepal® >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified  (discontinued **)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..