Petromont 3000 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Petromont
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 3000 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and other similar objects requiring rigidity, toughness and freedom from warpage.Petromont HDPE 3000 is a medium molecular weight homopolymer resin. Its very narrow molecular weight distribution and high density make it ideally suited for injection moulding applications where outstanding stiffness, warp resistance and toughness are demanded. Parts moulded from Petromont HDPE 3000 exhibit high gloss, low odour and are suitable for food packaging applications.
Physical Properties Metric English Comments
Density 0.965 g/cc
0.0349 lb/in³
ASTM D1505
ESCR 10% Igepal® 40 hour
40 hour
F<sub>50</sub>; ASTM D1693
Melt Flow 8.9 g/10 min
8.9 g/10 min
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Flexural Modulus 1.72 GPa
249 ksi
ASTM D790
Tensile Impact Strength 67.3 kJ/m²
32.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding