Dow Corning Q2-7735 ADHESIVE

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Q2-7735 ADHESIVE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Viscosity 30000 - 80000 cP
30000 - 80000 cP
dynamic
Thermal Properties Metric English Comments
Flash Point 27.0 °C
80.6 °F
closed cup
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+15 ohm-cm
2.50e+15 ohm-cm
Dielectric Constant 2.93

@Frequency 100000 Hz
2.93

@Frequency 100000 Hz
2.99

@Frequency 100 Hz
2.99

@Frequency 100 Hz
Dielectric Strength 58.54 kV/mm
1487 kV/in
Dissipation Factor 0.0025

@Frequency 100000 Hz
0.0025

@Frequency 100000 Hz
0.0046

@Frequency 100 Hz
0.0046

@Frequency 100 Hz
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 55-58
Appearance translucent