Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 9113 White 02 Rigid PVC, Molding, White 02

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9113 White 02 Rigid PVC, Molding, White 02.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Izod Impact, Notched 6.41 J/cm

@Thickness 6.35 mm
12.0 ft-lb/in

@Thickness 0.250 in
ASTM D-256
11.7 J/cm

@Thickness 3.17 mm
22.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 189 kJ/m²
90.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.00 °C
143.6 °F
ASTM D-648
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1450
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 32
Copyright © lookpolymers.com All Rights Reserved