Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.4 MPa | 4700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PD 20 TF Black Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Omni Plastics OmniTuff™ HPP TF40 Homopolymer Polypropylene Talc Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 20-1202 Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 30-2000 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in per min, tangent; ASTM D638 |
Network Polymers NPP 30-2000 TF33 Description: 33% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH042V Polypropylene, Homopolymer, Extrusion, Sheet COPYLENE™ CH042V is a polypropylene homopolymer resin often used in extrusion applications. Replacement alternative to Pro-fax® HL561KInformation provided by Phillips 66. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Rochling Engineered Plastics Polystone® P Polypropylene Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
PolyMirae Moplen EP332C Pipe Extrusion Grade Polypropylene Moplen EP332C is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP332C is a block copolymer appreciated by customers in the mar.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 330ºF Cure Temperature MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Flint Hills 23H2A Random Copolymer Polypropylene Features: Excellent clarity. Product does not contain animal derived components.Applications: Designed for Blow molding and Thermoforming - A replacement for PET, PS and PC high clarity applicatio.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
Hyosung Topilene HJ541CP PP HJ541CP High Isostatic PP Impact CopolymerApplications:Cap of pressure bottleCharacteristics:High stiffnessSlip propertyMedium impactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | ASTM D638 |
Hyosung Topilene HJ640A PP HJ640A Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 32.4 MPa @Thickness 3.20 mm |
4690 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Spartech GELOY SP-6730 Weatherable Sheet Description: Weatherable SheetGeloy is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Spartech PE4130 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Techmer ES Statiblend® 02036 Polypropylene Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 330ºF Cure Temperature MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | chs 2.0 in/min; tangent; ASTM D638 |
Diamond Polymers NPP30-3500G Homopolymer Polypropylene Granules Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
ExxonMobil Paxon™ AD60-007 Blow Molding Resin Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Dow H349-02 Polypropylene Homopolymer Resin H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D638 |
Amco PRIMATOP HDPE RP 004 Granular High Density Polyethylene HDPE RP 004 features small particle size and is used in plastic lumber extrusion.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | ASTM D-638 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | |
Asahi Kasei Thermylene® P-20TC-5100 Chemically Coupled Polypropylene Compound, 20% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 32.4 MPa | 4690 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S375D Thermoplastic Polyurethane Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |