Material Notes:
high melt strength general extrusion and molding grade of nylon 6Information provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183-A
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ISO METHOD 527
Elongation at Break >= 100 %
>= 100 %
ISO METHOD 527
Flexural Modulus 1.85 GPa
268 ksi
ISO METHOD 178
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ISO METHOD 180
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ISO METHOD 3146C
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 215 °C
419 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F