Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries 360 Surface Insensitive Instant Superglue General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in .. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries SuperGlue Ethyl 320 Very low viscosity for pre-assembled componentsMeets military spec Mil-A-46050C Type II Class I |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries SuperGlue Ethyl 325 Low-Medium Viscosity - General purposeMeets military spec Mil-A-46050C Type II Class I |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries SuperGlue Ethyl 395 General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (5 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 120SI Surface Insensitive (40 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 130 (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 140 (200 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 140 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 180 (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 180 MEDICAL DEVICES APPROVED (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180 - MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moistur.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 799 Cyanoacrylate, Surface insensitive PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Garlock 50 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Spartech Polycast UF4 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation Description: Tygothane® C-544-A I.B.: More flexible than many other reinforced urethane tubings, Tygothane® Pressure Tubing can be used in some of the most physically demanding applications,.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® 4013 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
3M Scotch® 3311 Foil Tape Scotch® Foil Tape 3311 is an aluminum alloy foil with a pressure-sensitive adhesive and paper liner. The aggressive rubber adhesive sticks well to most surfaces and the paper liner makes for conven.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® PRISM® 401 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® Prism® 4011 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |