Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1200 cP | 1200 cP | Part A |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 - 5000 cP | 1200 - 5000 cP | |
Ritelok TL42 Nutlock Anaerobic. Medium strength threadlocker for screws, nuts and bolts. Prevent corrosion, Vibration resistant, Dismantle using normal tools |
|||
Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | Thixotropic |
ND Industries NutGrade® 121 Removable Threadlocker A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th.. |
|||
Viscosity | 1200 cP | 1200 cP | Part B, RVT, #2, 20 rpm; TM R050-12 |
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11.. |
|||
Viscosity | 1200 cP | 1200 cP | |
Resinlab® TL5022 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Viscosity | 1200 - 2500 cP | 1200 - 2500 cP | |
Huntsman Araldite LZ 8001 A-80 Brominated Resin Weight per Epoxide (EEW, g/eq) 410 to 460. Max color is 2.Comments/Applications: Bis A epoxy 80% solids in acetone (18-21% bromine). For use in manufacture of thin laminates, prepregs and rigid la.. |
|||
Viscosity | 1200 cP @Shear Rate 100 1/s, Temperature 180 °C |
1200 cP @Shear Rate 100 1/s, Temperature 356 °F |
Melt |
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom.. |
|||
Viscosity | 1200 - 1800 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200 - 1800 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e.. |
|||
Viscosity | 1200 cP | 1200 cP | 1.3% NaCl added |
Solvay MACKADET® CA-ND Surfactant Product description: Mackadet CA-ND is a concentrated blend of mild surfactants for use as a base for high foaming surfactant systems. Mackadet CA-ND responds rapidly to viscosity building with the .. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8010 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8010 is a specialized stabilizer for polyurethane rigid foams. Due to its extremely good nucleating performance it is especially recommended for the production of foams with a very fine c.. |
|||
Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | |
Master Bond Mastersil 151 Two Component Low Viscosity Silicone Compound Master Bond MasterSil 151 is a two component, low viscosity
silicone compound for high performance potting and
encapsulation. MasterSil 151 is an addition cured system and does not require exposure.. |
|||
Viscosity | 1200 - 1500 cP @Temperature 23.0 °C |
1200 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV10MED Biocompatible One Component UV Curable Adhesive System Master Bond UV10Med is a one part UV type system for bonding, sealing and coating. It fully passes USP Class VI testing requirements and features good optical clarity and physical properties as well.. |
|||
Viscosity | 1200 - 1850 cP @Temperature 125 °C |
1200 - 1850 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-10 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-10 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Zircar Zirconia ZR-CEM Zirconia Cement Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi.. |
|||
Viscosity | 1200 - 5000 cP | 1200 - 5000 cP | Thixotropic |
Loctite® 222 Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
Loctite® 222MS Low Strength/Small Screw Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 1200 cP | 1200 cP | dynamic |
Dow Corning FLUOROGEL® Q3-6679 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure, solvent and fuel resistant.Information provided by Dow Corning |
|||
Viscosity | 1200 cP | 1200 cP | |
Dymax 3089 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 1200 cP | 1200 cP | Nominal |
Dymax Light Weld® 426 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Viscosity | 1200 - 1800 cP @Temperature 30.0 °C |
1200 - 1800 cP @Temperature 86.0 °F |
|
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |
|||
Viscosity | <= 1200 cP | <= 1200 cP | |
Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound AboTar 8101-8 is a 2-part tar-epoxy variable-ratio system. It is weather- and water-proof, flexible, and acid, alkali, and fuel resistant. It can be used neat or with sand or aggregates. Uses: Resu.. |
|||
Viscosity | 1200 cP @Temperature 177 °C |
1200 cP @Temperature 350 °F |
Typical |
Bostik 2305 Good Heat Resistance EVA Glue Stick Bostik 2305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock. |
|||
Viscosity | 1200 cP | 1200 cP | 2:1, B Side |
ACC EP JS EPI Engineered Polymers Joint Sealant EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot.. |
|||
Viscosity | 1200 - 1600 cP | 1200 - 1600 cP | |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Viscosity | 1200 cP | 1200 cP | Part A |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 cP | 1200 cP | Mixed |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 cP | 1200 cP | |
Resinlab® TL5042 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Viscosity | 1200 - 2200 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200 - 2200 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2090130P5 Pink Dielectric Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 1200 cP | 1200 cP | Part A, RVT, #2, 2.5 rpm; TM R050-12 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |