Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 82.0 °C | 180 °F | 77-88°C (170-190°F) Continuous Service |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries SuperGlue Ethyl 322 High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 160SI Surface Insensitive (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE 440 SERIES GEL advanced thixotropic formula is designed to polymerize instantly by absorbing surface moisture. The prod.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | |
Parker Chomerics CHO-FAB CFT Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | Deflection temperature; load unknown. |
Abatron AboCast 8-17/Abocure 8-17 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 123 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2103 C.I. is a smooth.. |
|||
Maximum Service Temperature, Air | <= 82.0 °C | <= 180 °F | Optimum performance range |
Sorbothane Polyurethane Damping Material, 30 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Westlake Plastics Propylux® Void-Free Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance to abrasion. These properties make it suitable fo.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Trelleborg Sealing Solutions HiMod® 912 Thermoplastic Bearing Thermoplastic BearingCharacteristics: HiMod® 912 was developed for application with intermittent temperature of 200°F, but requiring a more demanding bearing material with higher performance, imp.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® Super Bonder® 430 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
DIAB TBR® 10 Multifunctional Polymer Core Material TBR® is a multifunctional polymer core designed for hard points within sandwich structures where through-bolting or point-loading would normally cause local crushing of low density sandwich cores. .. |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | Long term |
3M 465 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | |
3M Scotch-Weld™ MG05 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | Long term |
3M 415 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | Long term |
3M 927 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer adhesion to a wide variety of surfaces, including many plastics. This pressure-sensitive medium firm acrylic adhesive family features a very.. |
|||
Maximum Service Temperature, Air | 82.0 °C | 180 °F | |
Parker Chomerics CHO-SHIELD® 1091 Adhesion Promoter for Conductive Polyurethane Coatings Information provided by Chomerics |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | >= 82.0 °C | >= 180 °F | |
Henkel Hysol EA 9320NA Paste Adhesive System High shear and high peel adhesive system with room temperature cure. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® 4541 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® Prism® 4011 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |