Parker Chomerics CHO-SEAL 1217 Conductive Elastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Parker Chomerics
Trade Name CHO-SEAL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL 1217 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.50 - 4.50 g/cc
3.50 - 4.50 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 80
70 - 80
ASTM D2240
Tensile Strength at Break >= 1.24 MPa
>= 180 psi
ASTM D412
Elongation at Break 100 - 300 %
100 - 300 %
ASTM D412
Tear Strength 6.13 kN/m
35.0 pli
ASTM D624
Compression Set <= 35 %

@Temperature 100 °C,
Time 252000 sec
<= 35 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flex TR10; ASTM D1329
Electrical Properties Metric English Comments
Volume Resistivity 0.010 ohm-cm
0.010 ohm-cm
as supplied without pressure sensitive adhesive; MIL-DTL-83528
<= 0.15 ohm-cm
<= 0.15 ohm-cm
Post Tensile Set; MIL-DTL-83528 Para.4.6.9
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
>= 110 dB

@Frequency 1.00e+10 Hz
>= 110 dB

@Frequency 1.00e+10 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 115 dB

@Frequency 2.00e+9 Hz
>= 115 dB

@Frequency 2.00e+9 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 120 dB

@Frequency 1.00e+8 Hz
>= 120 dB

@Frequency 1.00e+8 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 120 dB

@Frequency 5.00e+8 Hz
>= 120 dB

@Frequency 5.00e+8 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
Descriptive Properties Value Comments
Binder Fluoro-silicone
EMP Survivability >0.9 kA / in
MIL-DTL-83528 Para.4.6.16
Filler Ag/Cu
Heat Aging <0.015 ohm-cm
MIL-DTL-83528 Para.4.6.15
Type C
MIL-DTL-83528
Vibration Resistance, After <0.01 ohm-cm
MIL-DTL-83528 Para.4.6.13
Vibration Resistance, During <0.015 ohm-cm
MIL-DTL-83528 Para.4.6.13