Polymer Property : Shielding Effectiveness = 70 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 70 dB

@Frequency 1.00e+10 Hz
70 dB

@Frequency 1.00e+10 Hz
1/8 thickness
PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Shielding Effectiveness 70 dB

@Frequency 200000 Hz
70 dB

@Frequency 200000 Hz
Mil-G-83528/Mil std 285
P & P Technology EC-S Pure Silver Loaded Silicone
P & P Technology material reference EC-S is a silicone elastomer with Silver conductive filler. It is tan in color. The material is specially compounded to offer excellent physical and electrical p..
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer
High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer
Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat..
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer
Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip..
Shielding Effectiveness >= 70 dB

@Frequency 2.00e+9 Hz
>= 70 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 3, CHO-TM-TP09
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer
Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast..
Shielding Effectiveness >= 70 dB

@Frequency 1.00e+10 Hz
>= 70 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 3, CHO-TM-TP09
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer
Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast..
Shielding Effectiveness >= 70 dB

@Frequency 2.00e+9 Hz
>= 70 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 1, CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i..
Shielding Effectiveness >= 70 dB

@Frequency 1.00e+10 Hz
>= 70 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 1, CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i..
Shielding Effectiveness 70 dB

@Frequency 1.00e+10 Hz
70 dB

@Frequency 1.00e+10 Hz
2mm x 6mm
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket
Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t..
Shielding Effectiveness 70 - 80 dB

@Frequency 2.00e+7 - 1.00e+10 Hz
70 - 80 dB

@Frequency 2.00e+7 - 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket
Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t..
Shielding Effectiveness 70 dB

@Frequency 100000 Hz
70 dB

@Frequency 100000 Hz
H-Field
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout indu..
Shielding Effectiveness >= 70 dB

@Frequency 100000 Hz
>= 70 dB

@Frequency 100000 Hz
H-Field
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation..
Shielding Effectiveness >= 70 dB

@Frequency 100000 Hz
>= 70 dB

@Frequency 100000 Hz
H-Field
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by ..
Shielding Effectiveness 70 dB

@Frequency 1.00e+9 Hz
70 dB

@Frequency 1.00e+9 Hz
Plane Wave
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer
Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing...
Shielding Effectiveness 70 dB

@Frequency 1.00e+9 Hz
70 dB

@Frequency 1.00e+9 Hz
Parker Chomerics SOFT-SHIELD® 2000 Low Closure Force, Foam Core EMI Gasket
Description: SOFT-SHIELD® 2000 Series gaskets consist of silver-plated nylon yarn knitted as the outer layer over a highly compressible, thermoplastic EPDM foam core. Through a special treatment pr..
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DLT-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer
Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p..
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer
Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p..
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat..
Shielding Effectiveness 70 dB

@Frequency 1.00e+10 Hz
70 dB

@Frequency 1.00e+10 Hz
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding
Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C..