Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.30 - 4.50 g/cc | 4.30 - 4.50 g/cc | |
Reade Advanced Materials Iron Chromite (FeO·Cr2O3) A key source of chromium. The general specification is: SFSA 16T-67. A source of chromium metal, chromium chemicals, pigment, refractory mortars, and used as foundry sand.Information provided by Re.. |
|||
Specific Gravity | 3.50 - 4.50 g/cc | 3.50 - 4.50 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Specific Gravity | 3.50 - 4.50 g/cc | 3.50 - 4.50 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat.. |