Karina 67/200-D-IS-SD Clear PVC Compound

Category Polymer , Film , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 67/200-D-IS-SD Clear PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 69

@Time 15.0 sec
65 - 69

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 17.2 MPa
>= 2490 psi
ASTM D 638
Elongation at Break >= 150 %
>= 150 %
ASTM D 638
Descriptive Properties Value Comments
Application Skin
Clarity OK
ME 03