Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO SEAL SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TURBO SEAL SERIES 50 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting surfaces and will flex with minor flange movements. Provides resistance to low pressure immediately after assembly of flanges.Applications:Typically used as a form-in-place pump gaskets, thermostats, compressors, transmission housings & axle covers.Thixotropic nature reduces the migration of liquid product after application.Part Numbers for this data: 50-050, 50-300Information provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Brookfield Viscosity 275000 - 950000 cP
275000 - 950000 cP
RVT Spindle 7 @ 20 rpm
Mechanical Properties Metric English Comments
Tensile Strength 0.0965 MPa

@Temperature 18.3 - 149 °C
14.0 psi

@Temperature 65.0 - 300 °F
Steel-grit based; ISO 6922
Shear Strength 6.00 MPa
870 psi
ISO 4587; Lap, Steel - grit based
>= 5.00 MPa

@Temperature 22.0 °C,
Time >=86400 sec
>= 725 psi

@Temperature 71.6 °F,
Time >=24.0 hour
ISO 10123; Compressive, Steel pins and collars
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 33.9 °C
>= 93.0 °F
Processing Properties Metric English Comments
Cure Time 15.0 - 120 min
0.250 - 2.00 hour
Cure Time, Primed Surfaces
60.0 - 120 min
1.00 - 2.00 hour
Cure Time, Unprimed Surfaces
Descriptive Properties Value Comments
Appearance Purple
Chemical Resistance 100% Initial Strength Retained
Acetone at 22°C, at 500hrs
15% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
160% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
165% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
20% Initial Strength Retained
Gasoline at 22°C, at 500hrs
80% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
80% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
85% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
90% Initial Strength Retained
Ethanol at 22°C, at 500hrs
95% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
95% Initial Strength Retained
Acetone at 22°C, at 1000hrs
95% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
Composition Dimethacrylate ester