Material Notes:
BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding excessive shrinkage. Ideal for stretch forms, patterns, dies, molds, duplications, prototypes, etc.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.24 g/cc
2.24 g/cc
Brookfield Viscosity 20000 cP

@Temperature 23.9 °C
20000 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 87

@Temperature 23.9 °C
87

@Temperature 75.0 °F
Tensile Strength, Ultimate 42.7 MPa
6200 psi
Flexural Strength 53.8 MPa
7800 psi
Flexural Modulus 6.76 GPa
980 ksi
Compressive Strength 102 MPa
14800 psi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.9 °C
138 °F
Processing Properties Metric English Comments
Cure Time 960 min

@Temperature 24.0 °C
16.0 hour

@Temperature 75.2 °F
Pot Life 90 min

@Temperature 24.0 °C
90 min

@Temperature 75.2 °F
2 lb. mass
Descriptive Properties Value Comments
Machinability Good
Mix Ratio 100:10 by weight, 100:26 by volume, resin/harder