Polymer Property : Brookfield Viscosity = 275000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 275000 - 950000 cP
275000 - 950000 cP
RVT Spindle 7 @ 20 rpm
Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT
TURBO SEAL SERIES 50 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting surfaces and will flex with minor ..