Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Cure Time, Unprimed Surfaces |
Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT TURBO SEAL SERIES 50 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting surfaces and will flex with minor .. |
|||
Cure Time | 60.0 - 120 min @Temperature 120 °C |
1.00 - 2.00 hour @Temperature 248 °F |
|
Resin Technology Group DPE110698-1 Two component Potting Compound Resin Technology Group DPE110698-1 Two component Potting CompoundClear, fire retardant, low viscosity potting compound. |
|||
Cure Time | 120 - 120 min @Temperature 80.0 - 80.0 °C |
2.00 - 2.00 hour @Temperature 176 - 176 °F |
Average value: 120 min Grade Count:2 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Hand Dry |
Industrial Nanotech Nansulateâ„¢ GP Translucent Insulation Coating Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.NANSULATEâ„¢ liquid applied insulation is a prem.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Hand Dry |
Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATEâ„¢ liquid applied insulation is a premium industrial grade rust proofing protective .. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Surface Dry |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Functional cure |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads Information provided by ITW Devcon |
|||
Cure Time | 90.0 - 120 min @Temperature 121 °C |
1.50 - 2.00 hour @Temperature 250 °F |
|
Henkel Hysol EA 9896 WPP Peel Ply Pre-impregnated, nylon peel ply product supplied in film form. Specially designed resin system capable of curing at 250°F / 121°C. Compatible with state-of-the-art composite prepreg resin syst.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Tack-free |
Sika Industry SikaFlex 221 Fast Cure Polyurethane Sealant/Adhesive Sika 221 SikaFlex Fast Cure Polyurethane Sealant/AdhesiveThis versatile product is the most popular adhesive/sealant. It is an excellent adhesive/sealant and can handle many light bonding applicatio.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Optimum cure schedule, overnight at 75°F plus 150-200°F |
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2057/9 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Cure Time | 15.0 - 120 min | 0.250 - 2.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 515 Flange Sealant Anaerobic GasketingLoctite® 515 Flexible Cure Gasket Eliminator® Flange SealantMakes flexible gaskets for rigid machined flanges with less than 0.050" gap. Flexes with flanges that move in servic.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | light use |
3M 32662 Black Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Cure Time | 60.0 - 120 min @Temperature 25.0 °C |
1.00 - 2.00 hour @Temperature 77.0 °F |
demold time |
BCC Products Kwik Kast BC 8645 Urethane Casting BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing.. |
|||
Cure Time | 90.0 - 120 min | 1.50 - 2.00 hour | Time to Handling Strength |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Cure Time | 90.0 - 120 min | 1.50 - 2.00 hour | Time to Handling Strength |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Air Set prior to curin |
Aremco Ceramabind™ 542 High Temperature Inorganic Binder Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C). |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | light use |
3M 32665 Green Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | light use |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Cure Time | 60.0 - 120 min @Temperature 24.0 °C |
1.00 - 2.00 hour @Temperature 75.2 °F |
demold time |
BCC Products Kwik Kast BC 8001 Urethane Casting BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed.. |
|||
Cure Time | 60.0 - 120 min @Temperature 24.0 °C |
1.00 - 2.00 hour @Temperature 75.2 °F |
demold time |
BCC Products Kwik Kast BC 8002 Urethane Casting Kwik Kast II is an enhanced fast cast polyurethane tooling system. It has been reinvented for greater moisture resistance and improved filler suspension for easier premixing of the components. Kwik.. |
|||
Cure Time | 60.0 - 120 min @Temperature 24.0 °C |
1.00 - 2.00 hour @Temperature 75.2 °F |
demold time |
BCC Products Kwik Kast BC 8650 Urethane Casting BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl.. |
|||
Cure Time | 60.0 - 120 min @Temperature 24.0 °C |
1.00 - 2.00 hour @Temperature 75.2 °F |
demold time |
BCC Products LIK-WOOD BC 8007 Urethane Casting Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an.. |
|||
Cure Time | 90.0 - 120 min @Temperature 24.0 °C |
1.50 - 2.00 hour @Temperature 75.2 °F |
demold time |
BCC Products METAL-KAST BC 8010 Urethane Casting New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | 2-4 hrs Air Set; 1-2 hrs at 160°F |
Aremco Pyro-Putty™ 1000 High Temperature Ceramic-Metallic Putty, Aluminum Filled Ceramic and Aluminum-Filled, Two-Part, Water Based Paste.For Applications to 1/2" Thick.Repairs Cast Aluminum Parts to 1400°F |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | Tack-Free Time |
3M AC-350 Class B-1/4 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | |
3M AC-350 Class B-1/4 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Cure Time | 15.0 - 120 min | 0.250 - 2.00 hour | Full Cure |
Loctite® 574 Semi-rigid Cure Anaerobic Sealant Anaerobic GasketingLoctite® 574 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Fast curing, large gaps |
|||
Cure Time | 60.0 - 120 min | 1.00 - 2.00 hour | light use |
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |