Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M ScotchPad™ 802 Repositionable Tape Pad

Category Polymer , Adhesive
Manufacturer 3M
Trade Name ScotchPad™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M ScotchPad™ 802 Repositionable Tape Pad.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ ScotchPad™ Repositionable Tape Pad 802 are pre-cut pads composed of linered sheets of low adhesion tape and can be easily applied to a surface, removed, and reapplied to another resurface. The conformable acetate backing and Post-it® adhesive in these sheets give excellent long aging characteristics. The matte surface can be written on.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.20 MPa
754 psi
ASTM D3759
Elongation at Break 15 %
15 %
ASTM D3759
Peel Strength 0.01643 kN/m
0.09375 pli
Adhesion to Steel; ASTM D3330
0.03287 kN/m
0.1875 pli
Adhesion to Neenah Bond Paper; ASTM D3654
Descriptive Properties Value Comments
Adhesive Type Post-it low adhesion adhesive
Appearance Clear
Users viewing this material also viewed the following: