Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Opnyl OP6GF15 Nylon 6, 15% Glass Reinforced, Dry

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Ovation Polymers
Trade Name Opnyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Opnyl OP6GF15 Nylon 6, 15% Glass Reinforced, Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the measurements are done in dry and wet conditions. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm

@Thickness 3.17 mm
0.0010 - 0.0020 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
50 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
50 mm/min; ASTM D638
Tensile Modulus 4.80 GPa
696 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 150 MPa
21800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C

@Thickness 3.20 mm
392 °F

@Thickness 0.126 in
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved