Material Notes:
High Density Polyethylene - Halogenated FR compound with good impact resistance. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Melt Index of Compound 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 18.0 MPa
2610 psi
50 mm/min; ASTM D638
Elongation at Break >= 50 %
>= 50 %
50 mm/min; ASTM D638
Tensile Modulus 0.400 GPa
58.0 ksi
50 mm/min; ASTM D638
Flexural Strength 16.0 MPa
2320 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 0.320 GPa
46.4 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.869 J/cm
3.501 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0