Mechanical Properties Metric English Comments
Izod Impact, Notched 1.869 J/cm
3.501 ft-lb/in
ASTM D256
Ovation Polymers Nima™ HL 18400 HDPE
High Density Polyethylene - Halogenated FR compound with good impact resistance. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepa..
Izod Impact, Notched 1.869 J/cm
3.501 ft-lb/in
ASTM D256
Ovation Polymers Nima™ NH PA66UT Nylon 66
Polyamide 66 - Ultra Tough, Flame Retarded Non-Hal grade with excellent retention of mechanical properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humi..