Material Notes:
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 720 MPa
104000 psi
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
390 MPa

@Strain 0.200 %
56600 psi

@Strain 0.200 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
420 MPa

@Strain 1.00 %
60900 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
230 MPa

@Strain 0.200 %,
Temperature 200 °C
33400 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
295 MPa

@Strain 0.200 %,
Temperature 100 °C
42800 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 45 %
45 %
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Modulus of Elasticity 200 GPa
29000 ksi
RT
172 GPa

@Temperature 400 °C
24900 ksi

@Temperature 752 °F
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 100 °C
8.89 µin/in-°F

@Temperature 212 °F
17.5 µm/m-°C

@Temperature 400 °C
9.72 µin/in-°F

@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C
0.120 BTU/lb-°F
RT
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
RT
20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Chromium, Cr 17 %
17 %
Iron, Fe 71.3 %
71.3 %
Manganese, Mn 6.5 %
6.5 %
Nickel, Ni 5.0 %
5.0 %
Nitrogen, N 0.15 %
0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000700 ohm-cm
0.0000700 ohm-cm
RT