Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 720 MPa | 104000 psi | Outokumpu Typical, Hot Rolled Strip/Sheet (CPP); EN 10002-1 |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Tensile Strength, Ultimate | 720 MPa | 104000 psi | Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms. |
|||
Tensile Strength, Ultimate | 720 MPa @Temperature 315 °C |
104000 psi @Temperature 599 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Ultimate | >= 720 MPa | >= 104000 psi | |
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Tensile Strength, Ultimate | 720 MPa | 104000 psi | |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Tensile Strength, Ultimate | >= 720 MPa | >= 104000 psi | |
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |