Mechanical Properties Metric English Comments
Tensile Strength, Yield 230 MPa

@Strain 0.200 %,
Temperature 100 °C
33400 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Tensile Strength, Yield 230 MPa

@Strain 0.200 %,
Temperature 100 °C
33400 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Yield 230 MPa

@Strain 0.200 %,
Temperature 200 °C
33400 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms.
Tensile Strength, Yield 230 MPa

@Strain 0.200 %,
Temperature 100 °C
33400 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4529 Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield >= 230 MPa

@Strain 0.200 %
>= 33400 psi

@Strain 0.200 %
Minimum
Aleris Weldural Aluminum Alloy, 500 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..