Mechanical Properties Metric English Comments
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Temperature 100 °C
42800 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms.
Tensile Strength, Yield >= 295 MPa

@Temperature 100 °C
>= 42800 psi

@Temperature 212 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Temperature 870 °C
42800 psi

@Strain 0.200 %,
Temperature 1600 °F
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Tensile Strength, Yield 295 MPa

@Thickness 6.30 mm,
Temperature 204 °C
42800 psi

@Thickness 0.248 in,
Temperature 399 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Thickness 8.00 - 25.0 mm
42800 psi

@Strain 0.200 %,
Thickness 0.315 - 0.984 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Thickness 25.0 - 60.0 mm
42800 psi

@Strain 0.200 %,
Thickness 0.984 - 2.36 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Thickness 7.90 - 25.0 mm
42800 psi

@Strain 0.200 %,
Thickness 0.311 - 0.984 in
Typical Strength
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %,
Thickness 25.0 - 60.0 mm
42800 psi

@Strain 0.200 %,
Thickness 0.984 - 2.36 in
Typical Strength
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Tensile Strength, Yield 295 MPa

@Strain 0.200 %
42800 psi

@Strain 0.200 %
Typical
Aleris Weldural Aluminum Alloy, 500 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..