Old Hickory No. 6 Kentucky Ball Clay

Category Ceramic , Clay , Ball Clay
Manufacturer Old Hickory Clay Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Old Hickory No. 6 Kentucky Ball Clay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
No. 6DC is a highly kaolin clay that can be used as a filler grade material where presence of some 200 M quartz residue is not harmful. Applications can include a variety of refractory compositions as well as non-ceramic building products such as cement and fiberglass reinforced construction board.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
50% of particles less than
0.53 µm
0.53 µm
Median particle diameter
1.0 µm
1.0 µm
61% of particles less than
<= 5.0 µm
<= 5.0 µm
84% of particles less than
pH 6.0
6.0
Soluble Sulfates 50.0 ppm
50.0 ppm
Specific Surface Area 18.8 m²/g
18.8 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00307 GPa
0.445 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Thermal Properties Metric English Comments
Shrinkage 4.6 %
4.6 %
Cone 04, Linear Fired Shrinkage
5.5 %
5.5 %
Linear Drying Shrinkage
6.0 %
6.0 %
Cone 3, Linear Fired Shrinkage
8.0 %
8.0 %
Cone 11, Linear Fired Shrinkage
Component Elements Properties Metric English Comments
Al2O3 29.05 %
29.05 %
CaO 0.12 %
0.12 %
Fe2O3 0.99 %
0.99 %
K2O 0.52 %
0.52 %
Loss on Ignition(%) 9.39 %
9.39 %
MgO 0.25 %
0.25 %
Na2O 0.080 %
0.080 %
SiO2 57.07 %
57.07 %
TiO2 2.43 %
2.43 %
Descriptive Properties Value Comments
Absorption (%) 12.5
Cone 3, Fired
15.2
Cone 04, Fired
6.3
Cone 11, Fired
CEC/MBI (meg/100 ml) 7.5
Crude Color White
Filtration (ml) 25
Pyrometric Cone Equivalent (PCE) 32
Water of Plasticity (%) 30
Wet Sieve Residue (%) 1.05
Wet Sieve Residue, +200 mesh