Polymer Property : Modulus of Rupture = 0.445 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00307 GPa
0.445 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Old Hickory No. 6 Kentucky Ball Clay
No. 6DC is a highly kaolin clay that can be used as a filler grade material where presence of some 200 M quartz residue is not harmful. Applications can include a variety of refractory compositions ..