Material Notes:
AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and exceptional toughness. Applications include laminated film products or sealant layers in flexible packaging structures. AFFINITY FM 1570 polymer has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. AFFINITY FM 1570 polymer complies with FDA regulation 21 CFR 177.1520 c3.2a, which allows for its use in direct food contact applications.Film properties below based on a film thickness of 51 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
Thickness 51.0 microns
2.01 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 10.5.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 640 %
640 %
Film Elongation at Break, TD 670 %
670 %
Elmendorf Tear Strength MD 360 g
360 g
Elmendorf Tear Strength TD 760 g
760 g
Elmendorf Tear Strength, MD 7.10 g/micron
180 g/mil
Elmendorf Tear Strength, TD 14.9 g/micron
378 g/mil
Film Tensile Strength at Break, MD 51.4 MPa
7450 psi
Film Tensile Strength at Break, TD 43.9 MPa
6370 psi
Optical Properties Metric English Comments
Haze 4.9 %
4.9 %
Gloss 78 %
78 %
45°
Processing Properties Metric English Comments
Processing Temperature 100 °C
212 °F
Seal Initiation temperature