Huntsman Araldite HZ 3801 Water-Based Hardener

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite HZ 3801 Water-Based Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Base Resin is Polyamine adduct. Typical Solids Content 60%. Approx. equivalent weight 175.Comments/Applications: Viscosity Z5 - Z6. Coatings and floorings Good adhesion and performance on wet or damp concreteData provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.