Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Good weldability and metallurgical stability Good resistance to stress corrosion crackingInformation provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Tensile Strength, Ultimate 903 MPa
131000 psi
630 MPa

@Temperature 300 °C
91400 psi

@Temperature 572 °F
725 MPa

@Temperature 100 °C
105000 psi

@Temperature 212 °F
Tensile Strength, Yield 240 MPa

@Temperature 300 °C
34800 psi

@Temperature 572 °F
345 MPa

@Temperature 100 °C
50000 psi

@Temperature 212 °F
469 MPa

@Strain 0.200 %
68000 psi

@Strain 0.200 %
Elongation at Break 47 %
47 %
45 %

@Temperature 100 °C
45 %

@Temperature 212 °F
45 %

@Temperature 300 °C
45 %

@Temperature 572 °F
Modulus of Elasticity 195 GPa
28300 ksi
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 µin/in-°F

@Temperature 68.0 - 212 °F
17.3 µm/m-°C

@Temperature 20.0 - 500 °C
9.61 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 - 100 °C
0.108 BTU/lb-°F

@Temperature 68.0 - 212 °F
0.550 J/g-°C

@Temperature 20.0 - 300 °C
0.131 BTU/lb-°F

@Temperature 68.0 - 572 °F
0.620 J/g-°C

@Temperature 20.0 - 500 °C
0.148 BTU/lb-°F

@Temperature 68.0 - 932 °F
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 - 100 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
15.0 W/m-K

@Temperature 20.0 - 500 °C
104 BTU-in/hr-ft²-°F

@Temperature 68.0 - 932 °F
Component Elements Properties Metric English Comments
Carbon, C 0.010 %
0.010 %
Chromium, Cr 24 %
24 %
Iron, Fe >= 48.04 %
>= 48.04 %
As Remainder
Manganese, Mn 6.0 %
6.0 %
Molybdenum, Mo 4.5 %
4.5 %
Nickel, Ni 17 %
17 %
Nitrogen, N 0.45 %
0.45 %
Electrical Properties Metric English Comments
Volume Resistivity 0.000092 ohm-cm
0.000092 ohm-cm
Users viewing this material also viewed the following: