3M Fluorinert™ FC-72 Electronic Liquid

Category Fluid
Manufacturer 3M
Trade Name Fluorinert™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Fluorinert™ FC-72 Electronic Liquid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Fluorinert™ Liquid FC-72 is a non-conductive, thermally and chemically stable liquid ideal for many direct contact single and two phase low temperature heat transfer applications, in testing, power electronics and other electronic applications.Features and BenefitsThermal stabilityChemical stabilityWide liquid rangeNon-conductiveNarrow boiling rangeCompatibilityInformation provided by 3M
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
Liquid
Solubility in Water <= 0.00050 %
<= 0.00050 %
Solubility <= 7.0 ppm
<= 7.0 ppm
Viscosity 0.64 cP
0.64 cP
Absolute
Kinematic Viscosity 0.38 cSt
0.38 cSt
Molecular Weight 338 g/mol
338 g/mol
Vapor Pressure 0.0390 bar
29.3 torr
Surface Tension 10 dynes/cm
10 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 88.0 J/g
37.9 BTU/lb
Latent, at normal boiling point
CTE, linear 1560 µm/m-°C
867 µin/in-°F
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Liquid
Thermal Conductivity 0.0570 W/m-K
0.396 BTU-in/hr-ft²-°F
Liquid
Boiling Point 56.0 °C

@Pressure 0.101 MPa
133 °F

@Pressure 14.7 psi
Pour Point -90.0 °C
-130 °F
Optical Properties Metric English Comments
Refractive Index 1.251
1.251
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 1.75
1.75
Dielectric Strength 1.50 kV/mm
38.0 kV/in
0.1" gap
Chemical Properties Metric English Comments
Critical Pressure 18.3 bar
13700 torr
Estimated
Critical Temperature 176 °C
349 °F
Estimated
Descriptive Properties Value Comments
Color Clear, colorless