Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 60% of particles less than |
Old Hickory 54-S Kentucky Ball Clay This ball clay is a multi- purpose clay that has excellent pressing, extrusion, and casting qualities. It has a moderately fine particle size distribution and the high plasticity and dry strength is.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 60% of particles less than |
Old Hickory 56-SR Kentucky Ball Clay This is a kaolinitic clay with excellent extrusion and die pressing characteristics. It has some colloidal carbon content but only a moderate amount of shrinkage. This clay is suitable for a variety.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 52% of particles less than |
Old Hickory FC-340 Tennessee Ball Clay The FC-340 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous composition. It has excellent response to deflocculation and a very good casting rate whil.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 69% of particles less than |
Old Hickory M-23 Tennessee Ball Clay This is a very high quality porcelain grade ball clay. It has fine particle size distribution for excellent plasticity and strength in pressing or plastic forming application. the low Fe2O3 and TiO2.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 68% of particles less than |
Old Hickory MCB-11 Tennessee Ball Clay A clay with excellent kaolin content and virtually no carbon content. It is highly plastic with excellent fired brightness and is an excellent clay for a variety of ceramic glaze and porcelain compo.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 41% of particles less than |
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |
|||
Particle Size | 1.0 µm | 1.0 µm | at 80% distribution <1 to 5 microns. |
PolyChem Alloy 5004 Talc Nucleator Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weig.. |
|||
Particle Size | 1.0 µm | 1.0 µm | |
Poco Graphite ZEE-2 Ion Implant Grade Graphite ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro.. |
|||
Particle Size | 1.0 - 2.2 µm | 1.0 - 2.2 µm | d50 |
Magyar Aluminum ALOLT 60F Aluminum Hydroxide Fine Precipitated Type |
|||
Particle Size | 1.0 - 2.2 µm | 1.0 - 2.2 µm | d50 |
Magyar Aluminum ALOLT 60P Aluminum Hydroxide Fine Precipitated Type |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 13% finer |
Malvern Minerals Novacite® L-337 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 13% finer |
Malvern Minerals Novakup® L-337 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 86% finer than |
Imerys Bardenâ„¢ R Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 1.0 µm | 1.0 µm | 86% finer than |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 1.0 - 3.0 µm | 1.0 - 3.0 µm | Laser Diffraction D50 |
H.C. Starck High Vacuum 120 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | 2% |
SGL Carbon Group CF 1135 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | 2% |
SGL Carbon Group CF 3100 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | 1.0 µm | 1.0 µm | |
Solvay Chemicals Blanc fixe HD 80 Blanc Fixe HD 80 is the optimal extender for almost all applications in the production of paints and coatings and plastic. Furthermore, it is used as a chemical in lead acid batteries.Information pr.. |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | D50 Sedigraph |
Solvay SUPER CEROXâ„¢ 1663 Surfactant Description: Super Ceroxâ„¢1663 is particularly suited for the polishing of ophthalmic lenses (mass production and prescription) and optical lenses. Benefits: High polishing efficiency, Very high.. |
|||
Particle Size | 1.0 µm | 1.0 µm | Thin Section Crystal Size |
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 1.0 µm | 1.0 µm | Median |
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Size | 1.0 µm | 1.0 µm | @ 10% |
CIMBAR Gel Talc for Polyester Filler Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes.. |
|||
Particle Size | 1.0 µm | 1.0 µm | D50 |
CIMBAR FlexTalc® 610 Ultrafine Talc for TPO Applications Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta.. |
|||
Particle Size | 1.0 - 2.5 µm | 1.0 - 2.5 µm | MA147LFE |
C.O.I.M. FILCO® 650 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |