Polymer Property : Soluble Sulfates = 50.0 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Soluble Sulfates 50.0 ppm
50.0 ppm
Old Hickory No. 6 Kentucky Ball Clay
No. 6DC is a highly kaolin clay that can be used as a filler grade material where presence of some 200 M quartz residue is not harmful. Applications can include a variety of refractory compositions ..