Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Impact Grade
Manufacturer Nylene®
Trade Name Norpex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Flexural Yield Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 3.40 J/cm
6.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ASTM D648