Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TQ261F2 PA46-GF10

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TQ261F2 PA46-GF10.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Glass Reinforced, Heat Stabilized
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
dry; ISO 1183
Moisture Absorption 3.10 %
3.10 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa
16700 psi
dry; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
dry; ISO 527-1/-2
Tensile Modulus 4.50 GPa
653 ksi
dry; ISO 527-1/-2
Flexural Modulus 4.00 GPa
580 ksi
dry; ISO 178
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
dry; ISO 75-1/-2
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved