Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 3.40 J/cm @Temperature 23.0 °C |
6.37 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
Ineos B53-35H-100 HDPE B53-35H-100 is a high density polyethylene copolymer developed for injection blow molding. Zinc Stearate is incorporated in the formulation as a release agent. It is recommended for use in applica.. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0133 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0133 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM-D256 |
Braskem GP5550 HDPE High Density Extrusion Polyethylene GP5550 is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. Its applications .. |
|||
Izod Impact, Notched | 3.40 J/cm | 6.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |