Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 1.4 - 2.4 %
1.4 - 2.4 %
ISO 62
Water Absorption at Saturation 5.0 - 7.0 %
5.0 - 7.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0050 - 0.014 cm/cm
0.0050 - 0.014 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 169 MPa
24500 psi
ISO 2039-1
Tensile Strength at Break 160 MPa
23200 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 11.2 GPa
1620 ksi
ISO 527
Flexural Modulus 8.00 GPa
1160 ksi
ISO 178
Charpy Impact Unnotched 3.80 J/cm²
18.1 ft-lb/in²
DIN 53453
NB
NB
ISO 179/1eU
3.00 J/cm²

@Temperature -40.0 °C
14.3 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
4.50 J/cm²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
DIN 53453
1.10 J/cm²
5.24 ft-lb/in²
ISO 179/1eA
0.700 J/cm²

@Temperature -40.0 °C
3.33 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 130 °C
266 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V
550 V
CTI 100; IEC 112
Users viewing this material also viewed the following: