Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications... |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:.. |
|||
Tensile Modulus | 11.2 GPa @Temperature 100 °C |
1620 ksi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ASTM Data |
Dow Questra® WA206 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ASTM Data |
Dow Questra® WA551 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527 |
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Tensile Modulus | 11.2 GPa @Temperature 100 °C |
1620 ksi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-1/-2 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Modulus | 11.2 GPa @Temperature -140 °C |
1630 ksi @Temperature -220 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced 40% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RVL36SXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVL36SXS is a compound based on PA 66 resin containing Long Glass Fiber, PTFE. Added features include; Internally Lubricated. |
|||
Tensile Modulus | 11.2 GPa | 1620 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers. |