Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 1.5 - 2.2 %
1.5 - 2.2 %
ISO 62
Water Absorption at Saturation 6.0 - 8.0 %
6.0 - 8.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 152 MPa
22000 psi
ISO 2039-1
Tensile Strength at Break 72.0 MPa
10400 psi
ISO 527
Elongation at Break 4.2 %
4.2 %
ISO 527
Tensile Modulus 3.30 GPa
479 ksi
ISO 527
Flexural Strength 90.0 MPa
13100 psi
ISO 178
Flexural Modulus 3.10 GPa
450 ksi
ISO 178
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
DIN 53453
1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eU
1.40 J/cm²

@Temperature -30.0 °C
6.66 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
ISO 179/1eA
0.260 J/cm²
1.24 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 3146 DSC
Maximum Service Temperature, Air 130 °C
266 °F
Continuous; FRISETTA Test Method
Users viewing this material also viewed the following: