Material Notes:
High Impact Nylon (33% Glass Fiber)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 1.0 %
1.0 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 157 MPa
22800 psi
ASTM D638
Elongation at Break 4.0 - 5.0 %
4.0 - 5.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
1/8 in specimen; ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
420 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 198 °C
388 °F
0.125 in bar; ASTM D648