Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 216 °C | 420 °F | ASTM D3418 |
Nylene® 204 (HS) , Fast Cycle Nylon 6 Description: Nylene® 204 (HS) is a fast cycle, medium viscosity, nucleated nylon 6. 204 is UL approved and automotive approved. Information provided by Custom Resins.ALM, Nylene Canada, and Custom .. |
|||
Melting Point | 216 °C | 420 °F | ASTM D3418 |
Nylene® 321 (HS) Impact Modified Nylon 6 Description: Nylene® 321 (HS) is an impact modified nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D3418 |
Nylene® 4214-33 (HS) , 33% Glass Fiber Reinforced Impact Modified Nylon 6 Description: Nylene® 4214-33 (HS) is a 33% glass filled, high impact nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D3418 |
Nylene® Mach 6 , Fast Cycle Nylon 6 Description: Nylene® Mach is a fast cycle, high speed, high flow nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D789 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Melting Point | 216 °C | 420 °F | ASTM D789 |
Network Polymers Nylon 6015 G33HSL High Impact Nylon (33% Glass Fiber)Information provided by Network Polymers Inc. |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Melting Point | 216 °C | 420 °F | ASTM D3418 |
Quadrant EPP Quadrant Nylon 612 |
|||
Melting Point | 216 °C | 420 °F | |
Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 15% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized Appearance: BlackInformation provided by TP Compo.. |
|||
Melting Point | 216 °C | 420 °F | DSC |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
Melting Point | 216 °C | 420 °F | DSC |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
Melting Point | 216 °C | 420 °F | DSC |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D789 |
Plastics Group Polifil® 836L Nylon 6 (DAM) Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are appli.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D789 |
Plastics Group Polifil® 930L Nylon 6 (DAM) Polifil® NYLON 6 provides superior strength and rigidity with electrical resistance and surface lubricity.Applications: AutomotiveHousingsBearingsAppliances Standard processing techniques are appli.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D789 |
Plastics Group Polifil® 930L-13GF Glass Fiber-Reinforced Nylon 6 (DAM) Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind.. |
|||
Melting Point | 216 °C | 420 °F | ASTM D789 |
Plastics Group Polifil® 930L-33GF Glass Fiber-Reinforced Nylon 6 (DAM) Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in ind.. |
|||
Melting Point | 216 °C | 420 °F | |
Chase Plastics CP Pryme® N100HL (Dry) Nylon 6, Heat Stabilized, Lubricated Features: Heat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 °C | 420 °F | |
Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content Features: Heat StabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 °C | 420 °F | |
Chase Plastics CP Pryme® N340HL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated, Recycled Content Features: Heat stabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | Average value: 220 °C Grade Count:24 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |