Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LCF40-PA6 High Flow Nylon 6, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256-56 |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | 1/8 in specimen; ASTM D256 |
Network Polymers Nylon 6015 G33HSL High Impact Nylon (33% Glass Fiber)Information provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 2.24 J/cm @Temperature 23.0 °C |
4.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 2.24 - 7.4746 J/cm @Temperature -40.0 - -28.9 °C |
4.20 - 14.003 ft-lb/in @Temperature -40.0 - -20.0 °F |
Average value: 4.31 J/cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 2.24 J/cm @Diameter 3.17 mm |
4.20 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
Izod Impact, Notched | 2.24 J/cm @Diameter 3.17 mm |
4.20 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 6200 Super High Impact Polystyrene Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Izod Impact, Notched | 2.24 J/cm @Diameter 3.17 mm |
4.20 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 6201 Super High Impact Polystyrene Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |
|||
Izod Impact, Notched | 2.24 J/cm @Temperature -40.0 °C |
4.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Izod Impact, Notched | 2.24 J/cm @Temperature -40.0 °C |
4.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific) Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate.. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS PPE+PS blend. Unfilled. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific) Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 2.24 J/cm @Thickness 3.17 mm |
4.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V 500 ABS Medium Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® A100HH ABS Molding Resin, High Heat Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
Aclo Accucomp ABS ABS856BL High Flow Medium Impact Grade |
|||
Izod Impact, Notched | 2.24 J/cm @Temperature -40.0 °C |
4.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Chem Polymer Durlex 709 IH PBT, Impact Modified A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
Aclo Accucomp ABS ABS803L Medium Impact Grade |
|||
Izod Impact, Notched | 2.24 - 16.0 J/cm | 4.20 - 30.0 ft-lb/in | Average value: 9.69 J/cm Grade Count:26 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 2.24 J/cm @Temperature -40.0 °C |
4.20 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific) Medium heat, high impact PPO/HIPS alloy used in the automotive industry. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256A |
Braskem TI6350WV High Impact Copolymer Polypropylene Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for.. |
|||
Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Izod Impact, Notched | 2.24 J/cm @Thickness 3.17 mm |
4.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® SER20 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |