Nabaltec NABALOX® NO 713-10 Reactive Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Nabaltec GmbH
Trade Name NABALOX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec NABALOX® NO 713-10 Reactive Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insulationhigh mechanical strengthhigh temperature propertiesdimensional accuracyoptimized chemical resistanceRefractory Industry, Engineering Ceramics
Physical Properties Metric English Comments
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Density 2.35 g/cc
0.0849 lb/in³
Green Density
3.90 g/cc
0.141 lb/in³
3.92 g/cc
0.142 lb/in³
Sintered Density
Loss On Ignition <= 0.500 %

@Temperature 20.0 - 1100 °C
<= 0.500 %

@Temperature 68.0 - 2010 °F
Particle Size >= 0.50 µm
>= 0.50 µm
Primary Crystal Size
0.70 µm
0.70 µm
Specific Surface Area 7.0 - 9.0 m²/g
7.0 - 9.0 m²/g
BET
Thermal Properties Metric English Comments
Shrinkage 17 %
17 %
Sintering Shrinkage
Component Elements Properties Metric English Comments
Al2O3 >= 99.7 %
>= 99.7 %
Fe2O3 0.030 %
0.030 %
Na2O 0.10 %
0.10 %
SiO2 0.050 %
0.050 %
Processing Properties Metric English Comments
Sintering Temperature 1600 °C
2910 °F
Descriptive Properties Value Comments
alpha-Al2O3-Content % 95