SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa
11900 psi
ASTM D 638
Elongation at Break 3.3 %
3.3 %
ASTM D 638
Tensile Modulus 8.67 GPa
1260 ksi
50 mm/min; ASTM D 638
Flexural Strength 137 MPa
19900 psi
ASTM D 790
Flexural Modulus 6.29 GPa
912 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 3.82 J/cm

@Temperature 23.0 °C
7.16 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 223 °C

@Thickness 3.20 mm
433 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Users viewing this material also viewed the following: