Sintering Temperature 1600 °C

@Time 7200 sec
2910 °F

@Time 2.00 hour
Nabaltec GRANALOX® NM 9510 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 - 1700 °C
2910 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 - 1700 °C
2910 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Sintering Temperature 1600 - 1700 °C
2910 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9622 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 - 1700 °C
2910 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9816 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 - 1700 °C
2910 - 3090 °F
Interval (dense ceramic parts)
Nabaltec GRANALOX® NM 9916 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 °C

@Time 7200 sec
2910 °F

@Time 2.00 hour
Nabaltec GRANALOX® NM 9922 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Sintering Temperature 1600 °C
2910 °F
Nabaltec GRANALOX® NM 9922 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 °C
2910 °F
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Sintering Temperature 1600 °C
2910 °F
Nabaltec NABALOX® NO 613-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1600 °C
2910 °F
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1600 °C
2910 °F
Nabaltec NABALOX® NO 713-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Sintering Temperature 1600 °C
2910 °F
Nabaltec NABALOX® NO 713-40 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..