Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.35 g/cc | 0.0849 lb/in³ | Green Density |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Green Density |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Green Density |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Green Density |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Green Density |
Nabaltec NABALOX® NO 715-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Apparent |
Gouda Vuurvast AK 50 Dense Refractory Brick Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Apparent |
Gouda Vuurvast AK 44 Dense Refractory Brick Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Apparent |
Gouda Vuurvast AK 60 C Dense Refractory Brick Description: A bauxite based quality with a high abrasion resistance, successfully used in transition zones of rotary cement kilns.Remarks: This data represents average values, obtained from samples.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6 LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP YH0235AC PE LNP* Thermocomp* YH0235AC is a compound based on Polyester Elastomer containing a metal filler. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | |
UBE Tyranno Grade C Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | |
UBE Tyranno Grade S Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | |
UBE Tyranno Grade D Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Density | 2.35 - 2.55 g/cc | 0.0849 - 0.0921 lb/in³ | |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.35 - 2.45 g/cc | 0.0849 - 0.0885 lb/in³ | |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.35 g/cc | 0.0849 lb/in³ | Apparent |
Gouda Vuurvast AK 50 A Dense Refractory Brick Description: This brick has a low porosity and a high strength and therefore a very good slag resistance. Applications: rotary cement kilns.Remarks: This data represents average values, obtained fro.. |