Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 7.0 - 9.0 m²/g | 7.0 - 9.0 m²/g | BET |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 6.0 - 9.0 m²/g | 6.0 - 9.0 m²/g | BET |
H.C. Starck Grade HD 07 Boron Carbide, B4C Powder for hot-pressing.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltrat.. |
|||
Specific Surface Area | 6.0 - 9.0 m²/g | 6.0 - 9.0 m²/g | BET |
H.C. Starck Grade HP Boron Carbide, B4C Powder for hot-pressing.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltrat.. |